Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL PPX™ Resin PPX640F - Americas - (PPE+PP)-GF40 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL PPX™ Resin PPX640F - Americas:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Noryl PPX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
NORYL PPX™ 640F resin is a 40% glass reinforced alloy of polyphenylene ether (PPE) + polypropylene (PP). This injection moldable grade is NSF 61 certified and exhibits high elongation and stiffness along with temperature performance, impact resistance, hydrolytic and dimensional stability. NORYL PPX640F resin is an excellent candidate for copper and brass replacement in water management applications such as water filtration systems, boiler systems, and heat exchangers.

UL Yellow Card Link E121562-221228
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 1.3 g/10min ASTM D 1238
Temperature 260 °C -
Load 5 kg -
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength at Yield 95 MPa ASTM D 638
Tensile Strength at Break 95 MPa ASTM D 638
Elongation at Break 6.4 % ASTM D 638
Flexural Modulus 8310 MPa ASTM D 790
Izod Impact notched, 1/8 in 106 J/m ASTM D 256
Izod Impact notched, Low-Temperature 96 J/m ASTM D 256
Temperature -30 °C -
Izod Impact unnotched, 1/8 in 576 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Burning behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
ASTM Data
DTUL @ 66 psi 158 °C ASTM D 648
DTUL @ 264 psi 146 °C ASTM D 648
Vicat Temperature 163 °C ASTM D 1525
Other propertiesValueUnitTest Standard
Density 1300 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 65 - 75 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.02 % -
Melt temperature 260 - 305 °C -
Mold temperature 40 - 65 °C -
Zone 1 245 - 290 °C -
Zone 2 250 - 290 °C -
Zone 3 255 - 300 °C -
Screw speed 20 - 100 rpm -
Back pressure 0.3 - 0.7 MPa -
Characteristics
Processing
Injection Molding
Regional Availability
North America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.